![How to get rid of the convex bead on butt weld? Recently started MIG after switching from flux core. 0.025" wire, 2" square tubing with 0.100" wall. Lincoln 180. My fillet looks How to get rid of the convex bead on butt weld? Recently started MIG after switching from flux core. 0.025" wire, 2" square tubing with 0.100" wall. Lincoln 180. My fillet looks](https://i.redd.it/wb3vpbxa8g461.jpg)
How to get rid of the convex bead on butt weld? Recently started MIG after switching from flux core. 0.025" wire, 2" square tubing with 0.100" wall. Lincoln 180. My fillet looks
![JMMP | Free Full-Text | The Effect of Switchback Parameters on Root Pass Formation of Butt Welds with Variable Gap | HTML JMMP | Free Full-Text | The Effect of Switchback Parameters on Root Pass Formation of Butt Welds with Variable Gap | HTML](https://www.mdpi.com/jmmp/jmmp-03-00054/article_deploy/html/images/jmmp-03-00054-g001-550.jpg)
JMMP | Free Full-Text | The Effect of Switchback Parameters on Root Pass Formation of Butt Welds with Variable Gap | HTML
![Welded Plate and the geometry of the 10 mm plates butt welded with a... | Download Scientific Diagram Welded Plate and the geometry of the 10 mm plates butt welded with a... | Download Scientific Diagram](https://www.researchgate.net/profile/Owolabi-Biodun/publication/270475301/figure/fig1/AS:295110622367747@1447371263578/Welded-Plate-and-the-geometry-of-the-10-mm-plates-butt-welded-with-a-weld-gap-of-3-mm.png)